Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Bonding honeycombe
Bonding honeycombe
Post Reply
Like
3
Bonding honeycombe
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
ajb100
ajb100
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
lookin to make my first honeycombe panel and have been thinking about how to join the layers together.
The plan will be to infuse two sheets of carbon and then vag bag them onto the core. I've seen EC do an adhesive for bonding cores, but how's best to apply this? Do you just lay a big lump down and spread it out with a spreader? My other thought had been to just mix up more resin, maybe thicken it a little, and then paint that on to the carbon.
Any other ideas or input?
Reply
Like
3
Reply
scottracing
scottracing
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
if you can get some film adhesive, its made for this job. you will need to cure at temperature though, so not sure if thats possible in your case?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Bonding honeycombe
ajb100
-
9 Years Ago
Both will work, personally I prefer using epoxy with a bit of fumed silica. Adhesive ends up a bit...
Hanaldo
-
9 Years Ago
if you can get some film adhesive, its made for this job. you will need to cure at temperature...
scottracing
-
9 Years Ago
Thanks for the replies. Cost is an issue on this so thickened resin it is I can heat cycle for an...
ajb100
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search