I need a prepreg film much like the kind used on the EC prepreg surface layer, except without the carbon.  
Purpose is for use with wood veneers, to add thickness to existing prepress for polishing and pinhole prevention.

Any ideas on where one can get such a material?

Any other suggestions for pinhole free OOA prepreg would be appreciated. 
Reply
morepower
morepower
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
Cytec do a resin film and so do SHD Composites. But I am not sure it would help much. If it is on the surface you may still have surface issues as it does not always work how you expect. I tried some a couple of years ago hoping the extra resin would stop pinholes. Sadly it did not and the results were possibly a little worse at best there was no difference. 