XCR Skinning process


Author
Message
Lenny
Lenny
Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)
Group: Forum Members
Posts: 16, Visits: 58
I would like to carbon skin a part and I have a question regarding the 'tack' time before applying the carbon.  The part I want to skin is quite large and has complex surfaces.  I don't want the resin base coat to be really tacky as once you lay the carbon it is very difficult to manipulate into position within damaging the weave pattern.   Therefore, could you lay the carbon earlier, so that the base coat is not so tacky and allows you to manipulate the carbon ? The process states 1-2 hours, but laying on after 10-30 minutes, would this cause any issues ?
Reply
Lenny
Lenny
Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)
Group: Forum Members
Posts: 16, Visits: 58
I tried to download the instructions for the new XCR skinning process, but the address doesn't seem to work.

Not sure how specific they are compared to the general instructions provided on the starter kit page and using the mix ratio on the bottles.

Just wanted to make sure I'm not missing anything.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Lenny - 10 Years Ago
matthieutje65 - 10 Years Ago
Warren (Staff) - 10 Years Ago
Matt (Staff) - 10 Years Ago
67redrocket - 10 Years Ago
Dravis - 10 Years Ago
Lenny - 10 Years Ago
Warren (Staff) - 10 Years Ago
Warren (Staff) - 10 Years Ago
JonS - 10 Years Ago
Warren (Staff) - 10 Years Ago
JonS - 10 Years Ago
Dravis - 10 Years Ago
Dravis - 10 Years Ago
Warren (Staff) - 10 Years Ago
Davidcorrado - 10 Years Ago
Warren (Staff) - 10 Years Ago
meir - 10 Years Ago
Davidcorrado - 10 Years Ago
Davidcorrado - 10 Years Ago
Warren (Staff) - 10 Years Ago
Davidcorrado - 10 Years Ago
Warren (Staff) - 10 Years Ago
Umut Can Kizilray - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search