External epoxy covering of EPS


Author
Message
flyerdave01
flyerdave01
Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)
Group: Forum Members
Posts: 3, Visits: 5
Is there an epoxy resin suitable as an external waterproof and hard surface coat that will provide a decent finish on EPS?
Fasta
Fasta
Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K


I think there may a be a number of epoxy resins that give a decent and hard finish. 

But I feel generally that epoxies are mostly not much good for UV/gloss retention so a gloss finish will not stay glossy for long if exposed to much sun.




Edited 10 Years Ago by Fasta
flyerdave01
flyerdave01
Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)
Group: Forum Members
Posts: 3, Visits: 5
Hi

Thanks for your reply.

Can i ask in the light of what you say, what would you recommend I use?

 
Fasta
Fasta
Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
You have to use epoxy to start with since this is the only resin that will work on top of polystyrene foam. The polyester/styrene based resins will dissolve the foam.

Once it's coated with the epoxy (with or without glass?) then you could use other resins, I would consider the Duratec Sunshield. It's UV and specifically made to coat over epoxy or other resins. If you want a clear?

If you don't need clear then it could be coated over the epoxy coat with with a polyester flow coat to any colour you need. Tough and durable. You might want to do your own small sample just to test the adhesion between the epoxy and a polyester.




Edited 10 Years Ago by Fasta