Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Fiber pattern in mould surface after post cure
Fiber pattern in mould surface after post cure
Post Reply
Like
2
Fiber pattern in mould surface after post cure
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
67redrocket
67redrocket
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 486
I have done a couple of attempts with a mold i created with the uni-mold. The mold was not post cured. When i make parts that is not post cured there is no problem, but when I create parts that i post cure i get a carbon fiber pattern in the mold surface. This pattern I have to sand down with 1200 paper to get it flat after I demold the part.
Is this happening because I did not post cure the mold? Do I have to make a new mold?
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Fiber pattern in mould surface after post cure
67redrocket
-
8 Years Ago
You should always post cure above the temperature that you cure at, sounds like the gel coat is...
racecomp
-
8 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search