Hi,

I am planning on making a small (approximately 1m x 0.5m x 0.5m) hull for a vehicle, but is effectively a boat hull with no contours just straight (tapered) sides out of glass fibre. I will only be making one model and have limited time, so rather than manufacturing a plug of the intended shape out of polyurethane then using the uni mould system to create the mould for the hull, is it possible to just create the inverse shape of the hull out of polyurethane (or another material) and cover it with (I think) a protective resin and a gel coat. I could then just hand lay up the fibres within this mould, would this be possible?

I guess the other option would just to make a male mould of the product and lay up around that (although I do appreciate the surface finishing would then be on inside). I would very much appreciate any help I can get on this matter.

See attached for the rough shape of the final required product (note it is upside down).

Many thanks

A
Attachments
Last years carbon fibre hull.jpg (530 views, 193.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search