Surface requirement for mould making


Author
Message
FLD
FLD
FLD
posted 8 Years Ago HOT
Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I mould from primered surfaces (2 pack) and I find the primer takes a sprayed coat of PVA release nicely to give a gloss finish.  Wax will give you a near gloss finish that's easy enough to polish up.  I found easylease didn't work well on primer; it seems to soak in and not act as a good release agent.  Might just be my experience.  Hope this helps.
Warren (Staff)
Warren (Staff)
Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8K
Professionally sprayed primer from a 2 pack system will usually be fine once fully cured.  You should get a release with any decent release agent. Ideally from a mould preparation point, it would be more convenient for a high gloss painted finish (2 pack also) as it means less work needed to finish the mould surface off to a high standard. However, if you don't mind polishing up the surface then you should be fine.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Makerbot
Makerbot
Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)
Group: Forum Members
Posts: 8, Visits: 126
Hi,

I am planning on making some car panel moulds, can you tell me if I can make the mould from panels in primer or do they need to be painted?

Thanks