Jacopo Carbonio
Jacopo Carbonio
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 43,
Visits: 109
Hi everyone
As I said in the title, I'm trying to build an oven for composites with some parts of my old house oven.
Some time ago I saw @Darren (Link topic:
http://www.talkcomposites.com/16787/Oven-build)
building an oven, and I would like to build something similar..so the question is..do you think I could use some parts of this?
I will need help for the electrical part of the work
Wainting your opinion, have a good day
Attachments
IMG_20151204_180848.jpg
(
974 views,
2.00 MB
)
IMG_20151204_180946.jpg
(
955 views,
1.00 MB
)
Reply
Like
5
Reply
Davidpetty1988
Davidpetty1988
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 26,
Visits: 89
Hi am loving the idea of a homemade composites oven
I got given an old oven and have purchased a pid temp controller
A k type thermocouple and a SSR and also a 1500watt element.
I will be doing prepreg vacuum parts in it what else do I need to complete my oven many thanks in advance
Dave
Tags
Oven
prepreg
Edited
9 Years Ago by
Davidpetty1988
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Building composites oven from old house oven
Jacopo Carbonio
-
10 Years Ago
Che bello non esser cagato da nessuno :rolleyes:
Jacopo Carbonio
-
10 Years Ago
I have seen several functional composite oven builds, made from "hot-air type" old kitchen ovens .....
Dravis
-
10 Years Ago
Hi am loving the idea of a homemade composites oven I got given an old oven and have purchased a pid...
Davidpetty1988
-
9 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search