Stevezx7r
Stevezx7r
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 6,
Visits: 52
Hi all, I've been having a look on the site at the various kits etc but before I get any further I have a quick question. I'm thinking of making a petrol tank for my bike - what would I need to do for this? I'm assuming I'll need some sort of iner tank or can fuel mix with carbon safely? Has anyone else gone this route before?
Thanks in advance!
Reply
Like
3
Reply
morepower
morepower
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
I use a phenol novolac sealer which is from a UK based company and is apparently a higher Phenol Novolac content than most which have been blended to reduce some of the costs. I am not sure how much there is in Caswell tank sealer but it is more expensive than I pay as I go straight to the supplier who makes blended resins. The trouble with pour and slosh coating is both wastage and possibly having the sealer slump and not fully coat the inside. I paint mine onto the inner sections before I bond them together and I use an adhesive I make which is based on the same resin. This allows me to alter the resin with thickeners and additives to make the adhesive or sealer work how I want. It is not a cheap resin to buy but I would say I can do 3 fuel tanks with 1.25Kg (resin and catalyst total weight). So it is not too bad when you look at it per tank. If you are doing them to sell then obviously you would be buying 5 or 10Kg so would get a better price too.
Aprilia RS250
Aprilia Falco fuel tank...
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Fuel tank question.
Stevezx7r
-
10 Years Ago
You need a special coating on the inside to be able to handle the fuels.
Hanaldo
-
10 Years Ago
Any idea what this coating is called? I suppose it'll have to be ethanol proof due to the amount...
Stevezx7r
-
10 Years Ago
Hi Steve, to quote Warren at Easy Composites [quote] Most epoxies have a good chemical resistance...
Rich (Staff)
-
10 Years Ago
Hmm, could be a PITA to source. Maybe a small Ali inner tank with a carbon dummy tank around...
Stevezx7r
-
10 Years Ago
Ethanol is the culprit,you can seal it with after you made the tank,using peel ply will give you a...
Shaneer22
-
10 Years Ago
You are in Europe, so the stuff you need is definitely available. Not sure what sort of quantities...
Hanaldo
-
10 Years Ago
Can I ask why you want to build a tank from CF, is it for looks or to lighten the bike. Its only...
VVS
-
10 Years Ago
[quote][b]VVS (12/09/2015)[/b][hr]Can I ask why you want to build a tank from CF, is it for looks...
Hanaldo
-
10 Years Ago
Kreem fuel tank liner is what myself and people I know use to coat our steel tanks. Just pour it in...
kidpaint
-
10 Years Ago
I would have thought a carbon tank would be stronger than the plastic one it has at the minute.
Stevezx7r
-
10 Years Ago
Strength can mean multiple things. Carbon is actually quite brittle, and failure is complete. So...
Hanaldo
-
10 Years Ago
I've seen (never used) rubber bladders for motorcycles. That might be an option if the...
speed_demon
-
10 Years Ago
I made a carbon tank for one of our race bikes and managed to get the weight down to 550 grams...
carbonfibreworks
-
10 Years Ago
https://www.aircraftspruce.ca/pages/cs/fueltanksealants/ps890.php > look in t Q&A section also...
20_rc51_00
-
10 Years Ago
I use a phenol novolac sealer which is from a UK based company and is apparently a higher Phenol...
morepower
-
10 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search