I have a requirement to apply a clear finish over a model yacht moulding in pre-preg.

In short, the moulding is in 1k carbon cloth, and the surface finish is not perfect by some margin. The strength, quality, and accuracy of the moulding is fine.... but the aesthetic finish is poorer than it should be.

The mouldings are exposed to sunlight from time to time, not on a daily basis, maybe a couple of days a week at the best. Some will be in hot countries with intense sunlight though.
They will not be exposed to significant scratching, unless rough handling or accident occurs. They will be placed in water for short periods, sea and river/lake (model yachts!).

So what I am looking for is a clear finish that can be flatted and buffed up to an excellent finish, that has some degree of UV stabilisation, is temporarily saline resistant, has a degree of scratch-resistance(although not essential) and forms a good bond with the pre-preg(assuming it's properly keyed).

My thoughts turn to a quality automotive 2k polyurethane clear coat.

But has anyone any experience of this? Or are there other alternatives?
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Depending on how much you will need to "even out" the surface, it will be a choice between 2-comp polyurethane or thicker layers of UV resistant Epoxy ..
However .. Epoxy will not polish up to a perfect "mirror finish"  .. so if yo do need a level of "filling" go for both.. First a layer of coating epoxy -- flatten that out, get a good even surface, then 2-comp clear coat.

That way you will get a perfect and very durable finish ..

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search