Can I ask why you want to build a tank from CF,
is it for looks or to lighten the bike.
Its only my personal opinion so what I know but I wouldn't want to crash a bike that had a tank made from CF, steel and aluminum tanks will deform and are very resilient to an off.
if you were under the bike and the tank split you'd be at risk of setting yourself alight, very nasty.
|