Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
With 20 pulls or so, the Mould itself may be wearing out and the surface may have become slightly damaged and hence the sticking. You can extend the life a little by using some pure silicone oil after each pull to restore any oils that dry out of the silicone.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|