Dear all,

I have some experience in hand laminating things and stuff with improvised molds and as next step I would like to do a glove box lid out of carbon fiber.
Until now I sprayd and sanded the part to get a nice surface - it is not perfect, nut I hate sanding and I will only give it a last polish.

My "big" questions are:
- regarding the part of the lock, is it realistic to close it with modeling clay without getting an undercut?
- what about the hinge. The original has a thin plastic as elastic hinge. I would prefer not to work with small metal hinges and I now in theory from rc-planes elastic hinges in FRP laminats using peal ply or aramid. If I do this, I need to extend the mould accordingly. What do you suggest?

Thanks a lot
Regards from Germany
Bernd
Attachments
IMG_5594_DxO.jpg (946 views, 236.00 KB)
IMG_5595_DxO.jpg (878 views, 348.00 KB)
IMG_5596_DxO.jpg (811 views, 275.00 KB)
IMG_5597_DxO.jpg (892 views, 372.00 KB)
Reply
Dravis
Dravis
Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Yes, the hinge can be made from Kevlar or Diolene fabric, and EF80 flexible resin from EC.

I have made several "protective" transport cases with this combination as a hinge.   One of them is now a few years old, and sees regular use, and it shows no sign of cracking or "fatigue"

In my case (pun intended BigGrin) the Case itself was done by infusion, and the hinge bonded on after making it with hand layup and vac bag,

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search