Looks like the one I have and mine works great. Keep in mind that an oil bath pump cannot run continusly or you will burn it out. A oiless vane pump are meant to run 24 -7 without problems, but you don't get as deep of a vacuum with these, my oilless pump gets about 26 HG the one like yours will go about 29.9 HG (full vacuum)