I'm looking for the fillet wax, but it would cost me ~£38 shipped or $68CDN!!!!! Anyone sourcing from a distributor in North America?
Reply
tomzi1234
tomzi1234
Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)
Group: Forum Members
Posts: 40, Visits: 500
This looks very similar.
i have filleting wax form EC, but from structure and smell defenetely looks beeswax.

so maybe anyone with no access to buy, could try this recipe.
http://craftingagreenworld.com/2011/...eling-beeswax/

i haven't try it. so don't get me wrong its 100% same

maybe it will help someone
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search