Gelcoat Gun Nozzle Size


Author
Message
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
Hi,
I have got a Gelcoat Gun and find it a bit like using a fire hose.
I am sure it is great for covering a large area but most of my moulds are only about 50mm wide but long.
I only use GC50 at the moment.
Has anyone tried smaller nozzles? If so what size?

Brian.
Reply
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Very clever!

Can you use the 3d printer to make a smaller nozzle for the gun? ๐Ÿ˜‰
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Brian_s - 10 Years Ago
Hanaldo - 10 Years Ago
MarkMK - 10 Years Ago
Brian_s - 10 Years Ago
VVS - 10 Years Ago
Brian_s - 10 Years Ago
AdamHutchin - 10 Years Ago
scottracing - 10 Years Ago
Hanaldo - 10 Years Ago
AdamHutchin - 10 Years Ago
George Sychrovsky - 10 Years Ago
Hanaldo - 10 Years Ago
Brian_s - 10 Years Ago

Similar Topics