Dravis
Dravis
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 592,
Visits: 1.9K
Brucecreations (01/07/2015)
[quote]
Yeah ... impressively WIDE Spread tow ... .. But the stuff on the hydrofoil, that has sort of a "hexagonal" pattern ... what fabric is that ??? It looks very nicely "high-tech"
The spread tow is delivered by easycomposites, the hexagonal one from an american company (If you need I can give you the link in PM).
Hi! Yes, I would like a link to the hexagonal pattern CF ...
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
Edited
9 Years Ago by
Dravis
Reply
Like
2
Brucecreations
Brucecreations
posted 9 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 25,
Visits: 371
Yeah ... impressively WIDE Spread tow ... .. But the stuff on the hydrofoil, that has sort of a "hexagonal" pattern ... what fabric is that ??? It looks very nicely "high-tech"
The spread tow is delivered by easycomposites, the hexagonal one from an american company (If you need I can give you the link in PM).
Almost too nice to use,
If it is pretty.. it works well
no words..incredible work and
incredible result man!!!
Grazie, 100% made in Italy
My You Tube Channel
Edited
9 Years Ago by
Brucecreations
Reply
Like
1
carbonfibreworks
carbonfibreworks
posted 9 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
Almost too nice to use, excellent quality .
Chris
Carbon fibre works LTD
Reply
Like
1
Dravis
Dravis
posted 9 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 592,
Visits: 1.9K
Yeah ... impressively WIDE Spread tow ... .. But the stuff on the hydrofoil, that has sort of a "hexagonal" pattern ... what fabric is that ??? It looks very nicely "high-tech"
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
Reply
Like
1
Jacopo Carbonio
Jacopo Carbonio
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 43,
Visits: 109
no words..incredible work and
incredible result man!!!
Reply
Like
2
Hanaldo
Hanaldo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Brucecreations (25/06/2015)
That is freakin massive spread tow carbon haha
I love the spread tow, I started with the 15 mm, but it wasn't enough, I used the 25 mm (changing the pattern from plain to twill....
) but I needed something more...
This one is 90 mm.... I think could be eonough..... for the moment.
I'm a big fan of spread tow, very unique fabric. Bit of a pain to work with, but it's worth it for the looks. Had no idea you could even get a 90mm, it's outrageous haha.
Reply
Like
2
davro
davro
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 300,
Visits: 2.2K
Inspiringly beautiful!
Can't wait to see your next cinematographic video of you surfing/flying this beauty
David Stevens
YouTube
: 
Comment | Rate | Subscribe
Instagram
Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale
Reply
Like
2
Brucecreations
Brucecreations
posted 9 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 25,
Visits: 371
That is freakin massive spread tow carbon haha
I love the spread tow, I started with the 15 mm, but it wasn't enough, I used the 25 mm (changing the pattern from plain to twill....
) but I needed something more...
This one is 90 mm.... I think could be eonough..... for the moment.
My You Tube Channel
Reply
Like
1
Hanaldo
Hanaldo
posted 9 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
That is freakin massive spread tow carbon haha... Is that what 24k looks like in that weave, or have you done something there?
As always, beautiful work.
Reply
Like
1
Brucecreations
Brucecreations
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 25,
Visits: 371
Thanks all!! And now I'm glad to show you my latest foil.
..
For those who like to see more pics , here
Google plus photo
you can found a lot
A new video coming soon
My You Tube Channel
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
4
Prev
1
2
3
4
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search