Adding to the points above, it can certainly help to use the heatgun to lift the bigger bubbles.
It is a bit of a fine art to find the right moment to lay the carbon. Too early is better than too late, as if you do it a bit too soon you can always wait until it tacks up properly. Some people find leaving the carbon in place for a bit longer before adding the clear resin can help too.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|