Hi

Within my company we use split fibreglass moulds to create plaster of paris core parts. Now these fibreglass moulds have become damaged along their joints and finishing the plaster has become a time consuming chore. The damaged areas can be around 3-4mm deep and a few inches long. I'd like to ask if Easycomposities can recommend a product that we could use to repair the damaged edges. 
I have tried to use Fast Cast resin but the moulds are not flat so I'd have to repair only small sections each time. We have the original wooden patterns (both inside and out) that can be used as a template to repair to. 
Ideally I'd like top place the wooden template inside the fibregalss mould and fill the damaged areas with a putty. Once it's hardened I could then remove the wooden template and dress the repair with abrasives.

I hope this all makes since. If not I will glad to try and clarify details.
The Fibreglass King
The Fibreglass King
Supreme Being (833 reputation)Supreme Being (833 reputation)Supreme Being (833 reputation)Supreme Being (833 reputation)Supreme Being (833 reputation)Supreme Being (833 reputation)Supreme Being (833 reputation)Supreme Being (833 reputation)Supreme Being (833 reputation)
Group: Forum Members
Posts: 69, Visits: 652
Hello Raz,
                    To be honest with you it sounds like you need to do some  proper repairs on your moulds, the problem with quick fix is they do not last and the damaged areas will increase costing you more time and money in the long run, In repairing your moulds and in finishing your products. As you are well aware your products are  only as good as the moulds when you break them out!  If you do not feel that you can do repairs yourself  I would be happy to sort them out for you as I run a F.R.P production moulding company and we offer a mould repair service both mobile and in house, If you are not to far from where we are based may be we could take a look at them for you?? 
Kind Regards
The Fibreglass King.....
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I would second what FK says and that a professional repair is the best route, repairing the fibreglass itself, then finishing with, if possible, the original gelcoat that was used.  If it is a polyester gelcoat then an additive such as Solution MW Wax Gelcoat Additive will help to stop the gelcoat curing tacky making it easier to sand flat and match with the rest of the mould when you finish it.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search