3D PET core resin uptake


Author
Message
Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Hey all, 

I'm just wondering if anyone has got specific data for the exact resin uptake of 3D PET core? Per m2/per mm thickness? 

Need to calculate my resin requirements for a job, roughly 1.1 sqm with 10mm PET core, but I can't find a specific number anywhere. 

Thanks a lot, 
Martin. 
Reply
Dravis
Dravis
Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
I did some tests some time ago, I will try to see if I can find some data for it ..

I infused 3 different core materials in the same go .. and cut out pieces of each in identical size .. I should be able to compute something from that..

Alternatively You can have the data, and work on them yourself... Cool

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)