Prepping a warped part for mould casting


Author
Message
Carbon Tuner
Carbon Tuner
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 104, Visits: 422
Well my next mould project is to create a front lip for the 2005-2009 Lotus Elise S2 USA version.


I ordered a fiberglass version to get the shape but I really want to make this part nice. As of now I have a perfect donor part, its just slightly warped. You can kinda see from the pic it does not sit flat, but it should!
http://www.talkcomposites.com/Uploads/Images/ab3461ce-5d58-4427-870d-d541.jpg

Any ideas on how I hold this down flat while I take a mould from it?


I'm using the mould for resin infusion. I really would like to attempt the lacquer coating technique, “like the pagani zonda”
Also, Anything I should do to the mold to prepare for this?

Then I may use the orginal part to try and modify the style a bit.


The ride:

http://www.talkcomposites.com/Uploads/Images/8baa9dad-383c-4a3f-a575-abfa.jpg










If Brute Force Isn''''t working your not using enough...
Edited 14 Years Ago by Carbon Tuner
Reply
Joe
Joe
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
When i fail I tell myself "Hey Joe, u just learned one way of NOT TO DO your part" BigGrin

For the board, i would primer/polish it too, i like to have consistent mold looking...but maybe I get picky.

Cheers.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search