Carbon fibre to carbon fibre bonding


Author
Message
Aysar
Aysar
Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)
Group: Forum Members
Posts: 3, Visits: 16
Hi

I am trying to bond a small piece of flat 2mm pre oreg carbon fibre to the side of a 5mm diameter carbon fibre rod and want to know what the strongest possible bonding method I should use.

The part once finished will have daily force put on it so really needs to be super strong.
I am considering using the ET-500 adhesive but not sure if that would be strong enough.

Any advice?

Thanks
Aysar
Reply
Aysar
Aysar
Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)
Group: Forum Members
Posts: 3, Visits: 16
Thanks everyone.

I have ordered the vudu glu and shall be testing it.

Thanks

Aysar
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search