Epoxy coating resin application
Epoxy coating resin application
Post Reply
Like
7
Epoxy coating resin application
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Maria Julia Ferreira
Maria Julia Ferreira
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 22
Hello,
I'm trying to apply an epoxy coating resin (bisphenol A epoxy resin) onto mild steel, with a bar coat of 100 micra. The resin to hardener ratio is 2:1.
When the surface begin drying some defects appear as the photo show. The surface preparation was done according to ASTM- G1- 03, and I tried to repeat the process with a bar coat of 200 micra and the result was the same.
What is wrong?
Can you help me?
Many thanks
Attachments
IMG_0472.JPG
(
1.1K views,
195.00 KB
)
Tags
epoxi resin problems
Edited
11 Years Ago by
Maria Julia Ferreira
Reply
Like
7
Reply
ChrisR
ChrisR
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
If the substrate is prepared correcting with no contaminants and it has been etched correctly then it will break down the surface tension of the epoxy and you will not get this fisheye problem. Therefore it must still have something on the surface and it hasn't been prepared correctly.
I have bonded steel (mild and stainless) into various resins, the only times I've had issues with bonding/wetting out has been when I haven't prepped correctly
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Epoxy coating resin application
Maria Julia Ferreira
-
11 Years Ago
From the photo it looks like the resin has "fish-eyed" off the surface due to the surface being...
Warren (Staff)
-
11 Years Ago
Thank you very much for your answer. But I have another doubt about the process: How much time...
Maria Julia Ferreira
-
11 Years Ago
I agree with Warren. What is the application? I'm assuming something for corrosion testing if you...
Hanaldo
-
11 Years Ago
Thank you for your suggestions. In fact, we are using this resin for anticorrosive tests. According...
Maria Julia Ferreira
-
11 Years Ago
My guess is you still have some form of contaminant / release agent / protective coating on the...
ChrisR
-
11 Years Ago
Thank Chris for your contribution. Anyway I hadit inconsideration regardingthe pre-treatment ofASTM...
Maria Julia Ferreira
-
11 Years Ago
If the substrate is prepared correcting with no contaminants and it has been etched correctly then...
ChrisR
-
11 Years Ago
Even the slightest trace of grease could cause that problem. Also if the surface is too smooth it...
Warren (Staff)
-
11 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search