I want to make a nose cone part (see attached), which I can make with a two part mould, but not sure how I would lay up and then vacuum bag such a deep part?

Can anyone suggest a suitable strategy for making this part? Or will I have to make the part in two halves and attach together?

Thanks!


Attachments
nose.jpg (239 views, 29.00 KB)
Edited 13 Years Ago by jamesw
neilb
neilb
Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)
Group: Forum Members
Posts: 107, Visits: 504
i'm guessing that it would have material on the bottom aswell?

i would make the mould in 3 pieces 1 on the left and 1 on the right as if it was a 2 piece mould (like you were thinking) then 1 on the bottom that way when you come to lay the fabric inside, you can leave off the bottom section and gain access to the rest of the mould with pro-finish carbon to get the visual effect, then bolt the bottom piece on and carry on laying up.
Edited 13 Years Ago by neilb
jamesw
jamesw
Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)
Group: Forum Members
Posts: 61, Visits: 558
Well the plan was to split the mould into a top and bottom half - but I'm still not sure how you would get it all sat correctly right to the end... I guess you would pressure bag the inside afterwards?

James
andygtt
andygtt
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
I laid the first layer of pro finish carbon into the moulds while they were speareted... and also a few of the following layers but clearly I left the joins in different possitions.... I then bolted the mould together and finished off on top of the existing layers fully but didnt need to be quite as careful to get weave perfect.

Of cause the issue you will also have is how do you smooth the bag out in this section as well... you need to be able to reach with your hand or risk voids on the bag anyhow.

rgds
Andy
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search