Group: Forum Members
Posts: 85,
Visits: 1.2K
|
I'm only using 30mm rock wool so 100mm is more than enough, if you're only taking the temperature up to about 80-100c then I wouldn't expect the heat transfered to be much? Best way is to just try it and monitor. If it becomes hot to touch redesign it, but I don't think you'll have a problem.
|