Clamping sleeve
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
joedusta
joedusta
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 2
Hi,
The closest ID~=OD (0.2mm) of your roll wrapped tube selection is
32.0mm (ID) / 34.8mm (OD)-(Inner tube) to
35mm (ID) / 37.8mm (OD) (Clamping sleeve). The plan is to cut a 2mm slot into the clamping sleeve and key in (with glue to adhere) m4 cf lugs that provide the clamping force. I have two possible approaches:
-Use the two tubes stated above and run the risk of being an extremely tight or loose fit (
Manufacturing Tolerance=
Inner Diameter: +/- 0.2mm:::
Outer Diameter: +/- 0.3mm
) therefore removing the advantage of using these two pipes. If both pipes are on opposite ends of the tolerance spectrum the risk is by the time sufficient clamping force is achieved by the clamping sleeve the sleeve has constricted too much thereby structurally damaging the cf matrix.
-Use the same tube (
32.0mm (ID) / 34.8mm (OD)
) as both the inner and outer and risk straining the sleeve getting it on and off.
What option should i take?
Is it possible for easycomposites member of staff to test the fit on a current batch? and provide me with those details so i can make an informed decision.
Regards
Joe
Tags
Clamping Sleeve Wrapped Tube Telescoping
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Clamping sleeve
joedusta
-
11 Years Ago
Either option will work fine. We normally would recommend not slotting the ends but purely bonding...
Warren (Staff)
-
11 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search