I have created a mould for a motorcycle seat, While I was releasing the former from the new mould i broke through the green gel coat where there was an air bubble.
Can I repair this with gel coat and repolish.
Reply
Chris929
Chris929
Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)
Group: Forum Members
Posts: 2, Visits: 3
Thanks 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search