pahanes
pahanes
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 29,
Visits: 20K
TomDesign (20/03/2015)
slushaj a kakoj lak ispolzoval? s pdnpvo kuska delal ili rezal okuratno i sprejam delal?
Clearcoat for car paint. Glasurit, brulex, spectral, dupont ... HS only.
Edited
11 Years Ago by
pahanes
Reply
Like
9
pahanes
pahanes
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 29,
Visits: 20K
Reply
Like
10
JasonH
JasonH
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 1,
Visits: 43
Really nice work.
I'm in the process of starting a project like this myself. Any tips or lessons learned you care to share? Also, what did you use to bond the two sides together, how many layers did you use and of what, and did you do any reinforcement to the areas where you mounted and support the window mechanisms?
Reply
Like
9
deceased10
deceased10
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 29,
Visits: 154
This is crazy! Great work! Do you happen to have any more pictures of the process! Really interesting stuff!
Reply
Like
10
DerekKarbonWorx
DerekKarbonWorx
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 4,
Visits: 13
what would a pair of these cost? in USD
Thanks
Derek
Reply
Like
9
kidpaint
kidpaint
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 99,
Visits: 676
When you made the inner brace, did you have to cut that out of the original door to make the mold of it? I have a brace that goes horizontally in a set of doors for me and feel that Im going to have to cut up a set of doors to make molds of them and would rather not since I had to have the doors sent over from Germany
Reply
Like
9
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Why would you need to cut it out of the door? It's the same process that EC cover in their making the bonnet tutorial. The inner skin mould is produced off the back of the outer skin mould.
Reply
Like
14
kidpaint
kidpaint
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 99,
Visits: 676
Sorry I didn't write that very well. I was meaning the vertical brace in the center of the door. Was that originally welded in and had to be cut out to make a mold? On my rs4 doors there is a brace thatbis welded between the inner and outer skin. Sorry I'm doing this on my phone so have to just paste a link. In the pic where the door is open you can see a brace going horizontally with 2 holes in it? I was wondering if yours was similarly welded in and you sacrificed the door after the outer mold was made to cut yours out and make a mold, or how I should attempt this.
http://www.audizine.com/forum/showthread.php/309855-So-you-want-to-do-an-RS4-Widebody-Conversion
Reply
Like
10
VVS
VVS
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Moderators
Posts: 226,
Visits: 334
Yes you would remove it but not cut it out, you would only drill out the spot-welds so causing very little damage.
when you take the mould you would then fill the drill holes with wax and leave a tiny indent that can then be used as marker points for drilling and fitting the carbon support.
very nice work.
Reply
Like
17
ChrisP
ChrisP
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 9,
Visits: 281
Great work and a great finish, what is the order of the stack of carbon fiber and are you using a vacuum regulator?
https://www.easycomposites.co.uk/smc-vacuum-regulator-for-vacuum-bagging
Chris
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
10
Prev
1
2
3
Next
Jump To Page
Similar Topics