ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
cant tell... but it can take quit a lot, depends on how thick you want it and for how much resin.
used it 50/50 in volume at some time...look for cotton flakes as well got a box of the brand west systems laying around somewhere, worked well
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
TomDesign
TomDesign
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Matt any info how much those things put into resin?
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
here are some links
with materials to thicken your resin
http://easycomposites.co.uk/products/resin-gel-silicone/fillers-and-additives/aluminium-tryhydroxide-filler-powder-for-casting-resins.aspx
http://easycomposites.co.uk/products/resin-gel-silicone/fillers-and-additives/glass-bubbles-microballoons-microspheres.aspx
http://easycomposites.co.uk/products/resin-gel-silicone/fillers-and-additives/fumed-silica-thixotropic-powder.aspx
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
TomDesign
TomDesign
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
what is that? any link?
Reply
Like
2
George Sychrovsky
George Sychrovsky
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 24,
Visits: 1.6K
Usually a mix of flox and silica
---------------------------------------------------------------------
Disclaimer opinions of others will vary depending on what they are selling
Reply
Like
3
TomDesign
TomDesign
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Guys what is used here from these guys for sharp egdes? they use same method for bodykit stuff also for the corners?
Thank you in advance
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search