ok i want to design and make my own custom molds but i have no idea how to or where to even start. do i make it out of wood first and go from there, or do i carve it out of clay or something. i have no idea. *sadface*

Can...you...DIG IT?!
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Building good usefull structures with "advanced Composites" like Carbon-fibre reinforced polymers is a Skill ... It must be aquired over a period of training, either on your own or through courses.

It helps immensely if you already have some skills in working with wood, metals or plastics. These skills will help you in making "Patterns", "Plugs" and moulds from existing parts.

To avoid costly mistakes, get some of the smaller "kits" from EC   and make some small parts first, using straight forward wet-lay and compress the layup with bags of sand, hot water (speeds up the cure a lot), shrink tape or other ways of compressing the pieces you make.

I "trained" a lot using just glass-fibre weave -- saves a lot of expensive CF ... Cool

Good luck!!

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search