I am beginning a series of projects that will involve carving into model board/foam board, to create relief wall panels. I want to carve them by hand, using something like a lino cutter. Can you recommend the best kind of board to use and do you have any knowledge about cutting tools I could use?

Thanks!
David
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
PU240 Medium Density Model Board is the densist model board i would choose for hand working.  You could go lighter but it will effect surface detail so it depends on the precision you need.

The board can be worked by hand with simple tools even down to sandpapers and sanding blocks.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Corby
Corby
Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)
Group: Forum Members
Posts: 3, Visits: 10
Great, thanks for your help. Can I use tools such as chisels and wood tools on this board?

David
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You can just be careful initially until you get the "feel" as foam behaves differently to wood.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Corby
Corby
Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)
Group: Forum Members
Posts: 3, Visits: 10
Thanks Warren