Hi all

attempting to repair my carbon bike frames chainstay (non-drive side). So far I have followed crack down through the chainstay and removed all delaminated carbon. There is now a nice 1" hole but the rest of carbon is solid. I have tried to cut in on either side of the hole using a fine rasp, so have a decent chamfer about 1 1/2" either side of the hole.

My plan was to just use multiple layers of Carbon Fibre 2/2 Twill 3k 195g, but having read a little more, I'm concerned this might not be enough to affect a decent repair, would I need to use some sort of UD fiber first?

Any advice gladly taken

Rod
Reply
carbonazza
carbonazza
Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)
Group: Forum Members
Posts: 1, Visits: 5
Hi Warren,

Another chainstay questions.

Something sharp hit my non-drive chainstay (see the attached picture).
It was planted at the bottom of the hit.

http://www.talkcomposites.com/Uploads/Images/4d6f6167-75b3-47b6-a3be-201f.jpg


The Fishing Pole repair kit, I ordered, arrived home yesterday. But I just found the forum now...

I clearly understand the repair is to be done at my own risk. 
But what would you advise from the picture?
Do I just sand it, and follow the video tutorials?

Knowing that it doesn't seem to have any other cracks than what we see here.
The frame is unpainted carbon.

Cheers,