The pattern coat primer is already very dark grey  ????

It is a polyester based filler type coat ..   So ... Polyester pigments should work ..
 

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
duke
duke
Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)
Group: Forum Members
Posts: 10, Visits: 114
Hello,

I'm trying to find the suitable pigment to use with the pattern coat primer?
Polyester or expoy based pigment?