Boat Hulls


Author
Message
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Following repairing a skiff recently I've been asked a couple of times about boats.  Random!  The skiff was grp with a foam core.  Has anyone here made a boat before?  I'm curious about what sort of layups / thicknesses I'll find.  One of my enquiries was about experimenting with hull shapes on a powerboat so I'll guess thats a fairly robust layup!
Reply
Zorongo
Zorongo
Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)
Group: Forum Members
Posts: 40, Visits: 330
You should better let us know a bit more.
Mainly boat´s size (small may vary from one person to another, from 6 to 12 m ?)
Max speed, as it give pressure on the hull when striking the waves and so the stresses criterion for calculations..
Type of construction, sandwich, solid, exotics, glass.

Long time ago there was a thumb rule for solid hulls: 1 mm thickness per hull´s meter long. (10 m => 10 mm)

Now everything is better known and understood, allowing

A general use is to alternate woven roving and CSM as CSM ir resin rich and assurees a good interface between w roving

Cutting a sample or drill to builld same thickness is a good starting point.

Also depending on hull´s area, stresses vary a lot, from low on the sides to very high on the slamming area (where it hits the waves)

Same for local stresses, specially on sandwich construction, as core may collapse and may be substitued by high density, wood or even solid.....

If high spped, the hull can also hit truncks or any other floating object, and kevlar is often choosed for outer layers.....



A 30 Knots 12 m boat solid laminate had about 8 mm skin with a panel size of about 1,0 x 0,5 m 
Panel size is vital ........... 

Is a wide field .......
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search