Hi there,

Having a little issue to make a cover, a real part to a steering wheel center. 

Considering that the mould will be to another part, I need do have extra 2mm max on the original part, so that the mould can be correct to create the cover. 

Skinning used to be an option, but I really want the best finish possible.

Is there any material to cover the part, do increase volume enough without causing any trouble with the gelcoat/epoxy?

Thanks in advance guys!Smile
neilb
neilb
Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)
Group: Forum Members
Posts: 107, Visits: 504
you could cover the piece in wax sheet, it comes in varying thicknesses.

i'm guessing you want to make a part to fit onto the original steering wheel trim
Blackpool
Blackpool
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 4, Visits: 13
That´s it neilb! Any kind of wax sheet or specific? 

That tip can be right on the money for me! Smile Thanks
SebRS
SebRS
Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)
Group: Forum Members
Posts: 29, Visits: 558
This is your solution!

https://www.easycomposites.co.uk/sheetwax

Regards,

Seb.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search