Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Layers of carbon for race car body panels
Layers of carbon for race car body panels
Post Reply
Like
5
Layers of carbon for race car body panels
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
duke
duke
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 10,
Visits: 114
Let's hear some opinions on number of carbon layers for non structural panels of a race car.
E.g. a front bumper and fenders. Need to be rigid enough for high speed but doesn't need to take any other forces as aero devices are fitted to the structure of the car.
Would e.g. 1 top layer 200 gram with a 2nd layer of 650 gram mat be sufficient?
Reply
Like
5
Reply
duke
duke
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 10,
Visits: 114
Thanks. What type of core would you use? E.g Lantor Coremat 1.4mm?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Layers of carbon for race car body panels
duke
-
11 Years Ago
2 layers of scrim ;) it all depends on the shape of the bodywork, you could quite easily get 1x90g...
ChrisR
-
11 Years Ago
Thanks. What type of core would you use? E.gLantor Coremat 1.4mm?
duke
-
11 Years Ago
Chris is bang on in our experience. Either a PVC core or Soric/3D core will work fine in 3mm...
Warren (Staff)
-
11 Years Ago
for my carbon body I used: 200g carbon surface layer 200g carbon soric core 2mm 200g carbon 200g...
andygtt
-
11 Years Ago
Thanks. How would the Soric core work in wet lay with vacuum bag? Or would an infusion layup be...
duke
-
11 Years Ago
I only do resin infusion but i can't think of a reason soric will not work with wet lay... if weight...
andygtt
-
11 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search