I'm thinking about building a carbon fibre Mirror dinghy


Author
Message
FLD
FLD
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I remember people experimenting with hull textures / finishes some years ago in racing kayaks.  At one point the regatta lake ended up with a film of oil folloing all the boats!  When waxes and treatments were banned people found a 1200 grit 'satin' finish was best.  It can be achieved with 1200 grit paper or scotchbrite pads.  I guess it works like the sharkskin swim suits.