Flexural test ASTM D790


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Was the data sheet for the raw fibre or a laminate?  most fibre data is raw.

Same with resins.

So the combined composite laminate will perform differently depending on resin, cure, preparation etc.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
duybk2501
duybk2501
Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)
Group: Forum Members
Posts: 1, Visits: 5
Hello everyone,

I am a new member, I am learning MS at Korea. In my work, I have tested carbon sheet (plain weave) 1mm thickness following ASTM D790 standards, dimension of the specimen was 50.8x12.7x1 mm and test on 25.4mm support span. The carbon sheet was T300 TORAYCA and flexural modulus they mention is 125 GPa. But in my result, I calculated the result always about 50~55 GPa, I don't know the reason why the result unequal too much with data sheet from the manufacturer. The forcing at breaks was 33~38 Kgf.

Does anyone do this test? Please help me.

Thanks and best regards.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search