Depends on the vest what type of kevlar is in it. Before i worked here, I stripped apart a few old British vests I had from my military time and extras from a surplus shop. The specific type I had was full of multiple layers of Plain weave Kevlar around 200gsm. You can get some good size pieces from them.
For what was £20 from a shop or free if you signed up, I got probably about 20sqm per vest.