Dissolving the PU foam on a solvent ?


Author
Message
Pertabolis
Pertabolis
Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)
Group: Forum Members
Posts: 17, Visits: 193
Hi

I was wondering if it was possible to dissolve the PU 80 low density model board in some solvents after having laminated a CF cloth around it ?

The idea would be to
- cut the foam to the target shape
- apply the epoxy/CF cloth
- dip the hole thing in a jar of acetone / other solvent



Thanks for your help !
P.
Reply
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Baja,

No need to apologise; I guessed as much and that is what the forum is here for after all.

Pierre, regarding your material choice, diolen will be problematic if your surface sanding will break down into the diolen. If it won't and it's just the edges then I think that, allthough a little more frustrating at the edges, you woud be able to work with it. If you think you'll sand down into the diolen on the surface then stay well clear, it would be very hard to deal with in this sense.

Best regards, Matt


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Pertabolis - 13 Years Ago
baja_patient - 13 Years Ago
Pertabolis - 13 Years Ago
baja_patient - 13 Years Ago
Pertabolis - 13 Years Ago
baja_patient - 13 Years Ago
Matt (Staff) - 13 Years Ago
baja_patient - 13 Years Ago
steveastroUK - 13 Years Ago
baja_patient - 13 Years Ago
                     Yeah, polystyrenes come in clear as well as expanded forms.
steveastroUK - 13 Years Ago
Pertabolis - 13 Years Ago
Pertabolis - 13 Years Ago
Matt (Staff) - 13 Years Ago
Pertabolis - 13 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search