White haze remaining after wetsand


Author
Message
Whitesol
Whitesol
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 7, Visits: 15
Hi guys,
Been skinning for quite a while but now I've stumbled onto something new. I was doing a pair of doorsills using 400 gsm cloth. I applied the first coat letting it go to a full cure and then applied the 2nd coat ( epoxy laminating resin + fast type hardner) with sanding cause I felt the first layer may have been too thin.

2nd coat went for a full cure and then I started wetsanding it ( 400 grid ) After getting it all even, I saw white marks all over the panels, nothing new but this time they remain visible :-( Wiped it down with acetone but even then I can still see them .. Do I need to sand down even more or did something go wrong here ? Please advise :-)
Reply
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
An even better way: don't let the first layer cure fully before applying subsequent layers. This will create a chemical bond.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...