Group: Forum Members
Posts: 592,
Visits: 1.9K
|
Welcome to the forum!
Yup .. Carbon Kevlar mixed cloth really will not be cut with a knife ... You need a set of shears that are "micro-serrated" so they will hold the tough kevlar fibres and slippery carbon, when cutting.
Vacuum is not the only way to ensure a good fibre to resin ratio, but in my opinion the easiest, and most effective ..
When skinning parts you do not really need to be concerned about the resin amounts ... but getting a void/bubble free layer of fabric properly draped on to a part is not easy, it takes patience and practise..
Good luck!
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
|