Hi All, new to the forum here Smile

I have only ever made small parts in carbon before but am thinking about making a bonnet. One quick question, is it worth shelling out for a vacuum infusion setup, or can I just lay carbon with a brush as normal? Are the results really that much better?
carbonfibreworks
carbonfibreworks
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hello Jackso11
Yes infusion is the way to go,I would recommend you make a few smaller parts to develop your skills and study the EC tutorial https://www.easycomposites.co.uk/learning/how-to-make-a-mould-for-a-carbon-fibre-bonnet

Chris
www.carbonfibreworks.co.uk

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
combustioncraig
combustioncraig
Supreme Being (414 reputation)Supreme Being (414 reputation)Supreme Being (414 reputation)Supreme Being (414 reputation)Supreme Being (414 reputation)Supreme Being (414 reputation)Supreme Being (414 reputation)Supreme Being (414 reputation)Supreme Being (414 reputation)
Group: Forum Members
Posts: 26, Visits: 46
Be sure to make sure you vacuum pump is appropriately sized to do the job.  My first attempt at resin infusion I used a 8cfm unit with low viscosity epoxy resin (adtech 820) and I pulled it across my 1mx1.5m test section in less than a min.  I wasn't prepared for that and ended up wrecking my first batch of parts.  Good luck and what type of car were you thinking about doing?    
wildcard
wildcard
Supreme Being (506 reputation)Supreme Being (506 reputation)Supreme Being (506 reputation)Supreme Being (506 reputation)Supreme Being (506 reputation)Supreme Being (506 reputation)Supreme Being (506 reputation)Supreme Being (506 reputation)Supreme Being (506 reputation)
Group: Forum Members
Posts: 40, Visits: 406
Vacuum assisted curing: vacuum bagging or vacuum infusion is best for the complex curves and shapes that may be in a hood. Just doing a wetlay without vacuum will most likely cause bridging on those complex curves. Also in an infusion setup you can use spray adhesive to make sure the carbon is laid in all of the curves. So, yes I believe you should buy or start building an infusion setup. Once you get it, start with small parts to get accustomed to the new process. 
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Definitely recommend going for infusion, and playing around with it a bit before attempting a bonnet. I think I jumped into it a bit quickly, expecting it to be as easy as the EC and other videos make it look. But there is a bit of a learning curve to it, I still haven't achieved a perfect finish straight out of the mold, but I'm getting there BigGrin

It is definitely better than wet-lay in my opinion, even if the material costs are a little bit higher.
Jackso11
Jackso11
Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)
Group: Awaiting Activation
Posts: 4, Visits: 12
Is this also the way to go to make spoilers?

I have finally got my workshop ready to start making parts and want to make bonnets and spoilers, but am open to making pretty much anything recommended to get my skills up to standard.

I am having difficulty getting my head around how to mould a supra style spoiler though, I don't want to make 2 halves that split over time with air/wind force.