Group: Forum Members
Posts: 237,
Visits: 4.8K
|
Don't do it !
Done lots of crash structures in F1 and thou your not going to see the forces we see if anything did happen its still going to be a fair bit of force
It "could" be done-but not easily
Two main problems for you are -
1-What ever your end design was just like every one else you have to crash test it to have proof of concept
2-Fitting, one of the main areas do design goes into intergration of the roll hoop into the main structure to spread the loadings.
Your existing chassis set up will be far from ideal and leads to a compromised composite structure before you even start
Composite structure can be very good in the initial crash,not very good in a secondary impact
|