I've made my own short "checklists" for the different processes in composites, with things like : What needs to be in the "stack" when doing wet lay with vacuum bagging.
What the different mixing ratios are for different resin/hardener systems e.t.c.
Timing sheets for things like "cure to a tack" for the tooling Gelcoats .e.t.c. Fortunately my workshop is very well "temperature controlled" being rather small, and extremely well insulated (Did it myself with 100 and 200 mm rockwool all around ... so its cheap to heat in winter, and easy to keep cool in summer. It very rarely drops below 18 deg. C and only occasionally gets above 22 in summer.)
This makes the "time-sheets" posted on my wall very usefull ..