Hi




Until now I have been using epoxy resin to infuse my parts at home but I now have the chance to use Crestapol 1250LV urethane acrylate resin which is the system we use at work.  My question is will this be compatible with the pro finish CF that is partially impregnated with a resin polymer?




I've asked easy comp's but as yet have no answer, I presume because its not a resin that's in everyday use.  Does anyone here know?




Reason I want to use it is that IMO its a better resin that's cheaper and gives a more flexible / resilient product which is perfect for larger infusions like bumpers, the cure time can be changed from a standard 2hr's to 5 mins and the viscosity can be changed with heat to get a better flow on more complex parts.




Any help would be greatly appreciated.
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
It's not likely that anyone here has used it either, but it might be worth a small trial run to see and report back on the results?
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
We have not used any urethane acrylate resins yet to test fabric compatability, however, We cannot forsee any problem with using our ProFinish Carbon Fibre 2/2 Twill.

The resin binder is epoxy based so what we expect would happen is that the binder will just be encapsulated by the fresh resin.  The quantity of binder is very small.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
with regards to surface finish, just make sure that the binder-side of the pro-finish stays inside the layup, not out towards the mould/gelcoat.

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
kei
kei
Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)
Group: Forum Members
Posts: 5, Visits: 31
Cheers for the replies guys, i'll give it a test at work then and report back,
kei
kei
Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)
Group: Forum Members
Posts: 5, Visits: 31
Right then, did a few tests at work and results are as follows.




Materials used;

200gsm pro finish cloth

200gsm woven glass

4mm soric core

1" woven tape

Crestapol 1250LV urethane acrylate resin




results;

200gsm PF cloth and woven cloth (1 layer of each)

Perfect wet out, very low amount of resin to material ratio, resulting in very thin flexible sheet.  Only downside is woven glass tried to delaminate as peel ply was removed.




200gsm PF cloth, layer of soric with picture frame of 3 layers of woven tape and final layer of 200gsm PF cloth 

Perfect wet out, very low resin to material ratio, giving good strong inflexible sheet.




200gsm PF cloth folded in half (resin side to resin side)

Perfect wet out, very low resin to material ratio, perfect bond, good cosmetic finish and only slightly flexible.




In all instances resin was fed along the centre line of the part so it would flow out to sides to a glass fibre csm resin break, flow was fast and infusion of a 20cm square part was approx. 3 mins, mix ratio was 2.5% accelerator G and 2.5% of hardener using non heated resin.  In a 13 degree environment on a cool aluminium bed the cure was very slow but as soon as the bed was placed in a 40 degree oven the parts all fully cured after 2hrs.




Still not sure why the woven glass tried to delaminate with the PF cloth at the edges, but with careful removal of peel ply was able to work round that.  All in all a good test and confirmed that 1250lv is a perfect resin to use, have also tried it in a previously used mold intended for epoxy, built in same way as the the easy comp bonnet video using tooling resin and black gel coat and no problems there, the part pulled out fine with no bonding or damage to the molds gel coat finish.




Only downsides to this resin system are the chemicals, the accelerator and hardener are both fairly dangerous items and both should be stored and handled in a safe manner and always kept apart until mixing.