Stitching Coated Kevlar Protective Patch Material


Author
Message
GraStuCo
GraStuCo
Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)
Group: Forum Members
Posts: 1, Visits: 3
Hi folks,

Any problems with hand-stitching the above material or is it not a viable option due to it's toughness?

I am quite clearly a newbie so please forgive the question.

Thanks
Reply
Dravis
Dravis
Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
It's no harder to hand stitch than thin leather or the Vinyl stuff you use for motorbike seats.

If you find it hard on your hands, go buy a "leather stitching glove" where they sell goods for leather crafts.

Do not use "knife point" leather needles, they will cut "slits" in the waterproofing backing material.

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search