Ok i am gonna try to explain this as best as i can.
What i am trying/want to do is extend the surrounding of the shift lever surrounding.
Here is a picture of what it looks like original
http://i39.tinypic.com/2z8rjnt.jpg

The silver area left and right of the shift lever is 1 part, then the ashtray above the lever is a 2nd part.
What i want to do is remove the ashtray, and extend the 1st part and give it a small upward curve.
And make something like this picture
http://i42.tinypic.com/34xev46.jpg

So the question is.
How would i go about creating a mold for this.
The original part is flat so getting that in a mold is no problem.
However the new none existing part is the challenge.

And are there any specific components to use for this kind of work?

Afterward i just do a CF finish( car interior is CF original anyway), which i am already familiar with.


Hope i am making sense.

Thanks
jay,
jay,
Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)
Group: Forum Members
Posts: 10, Visits: 28
ok get to a breakers yard of buy a new part ! the buy a glue gun and make some fiberglass sheet to make your exstensions . Get rid of the ashtray part then set about making the gauge holder with the fiberglass sheet then when complete bond it to the surround , Then theres several ways to make the mold and none of them will save time LOL my way would be to body fill and smooth all joining parts then use a 2k high build primer (i use reface )http://www.polyfibre.co.uk/index.php?sec=prod&prod=142  you can get a real good finish with it and when you wax it it wont stick plus there will be very little finishing work to your mold after apart from a good polish!

so going back once its primers and sanded use plasticine to creat the exstensions/returns then mold as per

regards jay
Tags
YvesT
YvesT
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 6, Visits: 20
Alright, thanks a lot.
That makes it clear on what to do.
Got plenty of time, so i am not worried there Smile
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search