I notice several people have asked about finishes for worktops and I believe you where looking into finding suitable products,can you tell me if you have made any progress.I notice there are several products available in america but nothing in the UK.
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
We have been testing different resins on and off for the last few months but as yet we have not found a perfect resin for the job.  We are getting closer but we cannot give any lead time as yet.

As soon as we find the right product we will be announcing it on the website.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant