You can use balsa in an open mould.  Lay up the outside part and let it cure.  Bond in the balsa and stand a weight on it then let that cure.  Finally lay up the outer skin.  A core really does add a lot of stiffness so I think its worth your time to try it.  I've used the 3mm PVC foam quite a lot and I was amazed at the difference it makes.